Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of EasyWood™ - PLA-W40 - Formfutura BV

Material Data Center offers the following functions for EasyWood™:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other EasyWood datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
Other Standards[S]
メルトフローレイト, MFI 4.5 g/10min
S: These properties are reported by the producer according standards that are different to our defaults.
機械的特性単位テスト基準
Other Standards[S]
曲げ弾性率 2584 MPa
曲げ強さ 59.6 MPa
S: These properties are reported by the producer according standards that are different to our defaults.
熱的特性単位テスト基準
ASTM数据
溶融温度 145 °C ASTM D 3418
その他の特性.単位テスト基準
密度 1200 kg/m³ ASTM D 792
機械的特性(ィルム)単位テスト基準
ASTM Data
引張弾性率, 平行 1930 MPa ASTM D 882
引張強度, 平行 71 MPa ASTM D 882
破断伸び, 平行 171 % ASTM D 882
特殊な特性
成形加工法.
Additive Manufacturing
納入形状.
Monofilament
な特性
Low Warpage
Certifications
Contains renewable resources
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.