Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1185 A WM - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1185 A WM:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
DESCRIPTION
Elastollan 1185 AWM is a polyether based TPU with plasticiser
for matt surfaces

SPECIAL PROPERTIES
excellent resistance to hydrolysis and good flexibility at
low temperature, resistance to microbiological attack,
good wear performance, high tensile strength, good damping behavior

TYPICAL APPLICATIONS
cable sheathing

OTHER HINTS
predrying: 2-3h at 100-110°C (air circulating oven) or
80-90°C (dehumidified air dryer),
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
機械的特性単位テスト基準
ISO データ
伸び率100%時の応力 7 MPa ISO 527
伸び率300%時の応力 13 MPa ISO 527
破壊応力 TPE 45 MPa ISO 527
破壊ひずみ TPE >300 % ISO 527
圧縮永久ひずみ 23℃, 24h 20 % ISO 815
圧縮永久ひずみ 70℃, 24h 35 % ISO 815
引裂強さ 55 kN/m ISO 34-1
耐摩耗性 40 mm³ ISO 4649
ショア硬さA 87 - ISO 7619-1
ショア硬さD 39 - ISO 7619-1
その他の特性.単位テスト基準
密度 1150 kg/m³ ISO 1183
機能
 せん断弾性率-温度. , Elastollan® 1185 A WM, (TPU-ARET), BASF PU
 応力-ひずみ. (TPE) , Elastollan® 1185 A WM, (TPU-ARET), BASF PU
特殊な特性
成形加工法.
異形押出成形.
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.