Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of EMERGE™ PC/ABS 7710 - (PC+ABS) - Trinseo

Material Data Center offers the following functions for EMERGE™ PC/ABS 7710:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Emerge datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 13 g/10min ISO 1133
温度 260 °C -
荷重 2.16 kg -
成形収縮率, 平行 0.5 % ISO 294-4, 2577
ASTM数据
メルトフローレイト, MFI 11 g/10min ASTM D 1238
温度 230 °C -
荷重 3.8 kg -
成形収縮率., 平行 0.005 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2560 MPa ISO 527
降伏応力 55 MPa ISO 527
降伏ひずみ 3.8 % ISO 527
破壊応力 45 MPa ISO 527
破壊ひずみ 43 % ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 40 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30゚C 15 kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C 50 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 14 kJ/m² ISO 180/1A
温度 -30 °C -
ASTM数据
引張弾性率 2620 MPa ASTM D 638
降伏応力 60 MPa ASTM D 638
破壊応力 48.3 MPa ASTM D 638
降伏点伸び 3.8 % ASTM D 638
破断伸び 65 % ASTM D 638
曲げ弾性率 2689 MPa ASTM D 790
曲げ強さ 96.5 MPa ASTM D 790
ロックウェル硬度 R 120 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 480 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 198 J/m ASTM D 256
温度 -17.8 °C -
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 77 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 88 °C ISO 75-1/-2
ビカット軟化温度, A 104 °C ISO 306
ビカット軟化温度, B 94 °C ISO 306
1.5mm厚さでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 1.5 mm -
厚さhでの燃焼性 5V 5VB class IEC 60695-11-20
試験片の厚さ 2.0 mm -
ASTM数据
UL94 燃焼性 V-0 - UL 94
追加試験片の厚さ 1.5 mm -
線膨張係数, 平行 68.4 E-6/K ASTM D 696
線膨張係数, 直角 68.4 E-6/K ASTM D 696
DTUL @ 66 psi 90.6 °C ASTM D 648
DTUL @ 264 psi 79.4 °C ASTM D 648
ビカット軟化温度 104 °C ASTM D 1525
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 2.86 - IEC 62631-2-1
比誘電率, 1MHz 2.8 - IEC 62631-2-1
誘電正接, 100Hz 40 E-4 IEC 62631-2-1
誘電正接, 1MHz 70 E-4 IEC 62631-2-1
体積抵抗率 >1E13 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
その他の特性.単位テスト基準
密度. 1180 kg/m³ ISO 1183
密度 1170 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 3 - 4 h -
樹脂温度 230 - 270 °C -
金型温度 60 - 90 °C -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
難燃.
な特性
Blending Resin
アプリケーション
IT/ビジネスマシーンズ, 電気電子, 医療の
領域別の利用可能性
ヨーロッパ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com