Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of EVASIN EV-4405V - EVAL - ChangChun Group

Material Data Center offers the following functions for EVASIN EV-4405V:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Evasin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 3.77 g/10min ASTM D 1238
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ASTM数据
引張弾性率 3414 MPa ASTM D 638
降伏応力 54.1 MPa ASTM D 638
破壊応力 41.7 MPa ASTM D 638
降伏点伸び 6.04 % ASTM D 638
破断伸び 225 % ASTM D 638
曲げ弾性率 3247 MPa ASTM D 790
曲げ強さ 88.9 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 8.29 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
溶融温度 168 °C ASTM D 3418
ガラス転移温度 57 °C ASTM E 1356
その他の特性.単位テスト基準
密度 1140 kg/m³ ASTM D 792
Moisture Content 0.3 % -
特殊な特性
成形加工法.
射出成形., Blown Film Extrusion, フィルム押出成形., Pipe/Tube Extrusion, シート押出成形., コーティング., 熱成形.
特殊な特性.
帯電防止., 紫外線安定化., 透明.
な特性
Barrier Properties, Good Adhesion, Heat Sealable, Copolymer, Random Copolymer
耐薬品性
Solvent Resistance, Oil Resistance
Certifications
Food contact, Food approval FDA 21 CFR
アプリケーション
電気電子, パッケージング
領域別の利用可能性
アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com