Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Evoprene® 093 - TPE - Alphagary

Material Data Center offers the following functions for Evoprene® 093:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Evoprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Note: mechanical properties were originally reported according to ISO 37. Comparison with data according ISO 527 seems to be acceptable in this case.

Abrasion DIN 53516 = 286 mm³

Service Temp Guide = -50 to +80 ºC

Thermoplastic compatibility: PP

Air age 14 days @ 70C (ISO 188):
     DeltaShore A = 0
     Tensile Srength = 103 %
     Elongation at Break = 102 %

Comment: Evoprene window gasket grade. BS 7412 dynamic dull finish.
機械的特性単位テスト基準
ISO データ
引張強度 6 MPa ISO 37
破壊ひずみ 450 % ISO 37
圧縮永久ひずみ 70℃, 24h 53 % ISO 815
圧縮永久ひずみ 100℃, 24h 65 % ISO 815
ショア硬さA 61 - ISO 7619-1
Other Standards[S]
伸び率300%時の応力 7.2 MPa ISO 37
引裂強さ 24 kN/m ISO 6383
耐摩耗性 286 mm³ DIN 53516
S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
Other Standards[S]
密度. 1090 kg/m³ ISO 2781
S: These properties are reported by the producer according standards that are different to our defaults.
特殊な特性
成形加工法.
射出成形.
領域別の利用可能性
北アメリカ., ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.