Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Hostacom G3 R05 105555 - PP-GF30 - LyondellBasell Industries

Material Data Center offers the following functions for Hostacom G3 R05 105555:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Hostacom datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Hostacom G3 R05 105555 is a 30% glass fiber reinforced PP homopolymer, with excellent stiffness, good dimensional stability and low creep under load at elevated temperatures. The product is available in black color, pellet form. This grade is delivered in 105555 color version.

This material is able to replace Polyamide glass filled compounds especially in structural applications. 
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 4 cm³/10min ISO 1133
温度 230 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 7100 MPa ISO 527
破壊応力 98 MPa ISO 527
破壊ひずみ 3 % ISO 527
シャルピー衝撃強さ, +23°C 50 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 11 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 8 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 168 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 145 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 160 °C ISO 75-1/-2
ビカット軟化温度, B 135 °C ISO 306
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 3.0 mm -
燃焼速度, FMVSS, 1mm厚 40 mm/min ISO 3795 (FMVSS 302)
電気的特性.単位テスト基準
ISO データ
体積抵抗率 >1E13 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
その他の特性.単位テスト基準
密度 1140 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
顆粒., 黒
特殊な特性.
熱安定化.
な特性
Creep Resistance, Homopolymer
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.