Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Inzea® F2 HTS 655 - (PLA+PSAC) - Nurel S.A.

Material Data Center offers the following functions for Inzea® F2 HTS 655:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Inzea datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
more information can be found in the following table
Rilsamid® Chemical Resistance
機械的特性単位テスト基準
ISO データ
引張弾性率 1550 MPa ISO 527
引張強度 38 MPa ISO 527
降伏ひずみ 9.5 % ISO 527
破壊ひずみ 11.5 % ISO 527
曲げ弾性率, 23°C 1450 MPa ISO 178
曲げ強さ 50 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 7.5 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 150 °C ISO 11357-1/-3
荷重たわみ温度, 0.45 MPa 75 °C ISO 75-1/-2
その他の特性.単位テスト基準
Moisture Content 0.5 % -
特殊な特性
成形加工法.
射出成形., Fiber Extrusion, フィルム押出成形., 異形押出成形., ブロー成形., 熱成形.
特殊な特性.
熱安定化.
な特性
Amorphous
Certifications
Contains renewable resources, Biodegradable, Food contact, 堆肥化可能 ISO 13432 (プロデューサー), 堆肥化可能 ISO 13432 (証明書)
領域別の利用可能性
ヨーロッパ., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.