Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KEBAFLOW LCP HF140 - LCP-GF40 - Barlog plastics GmbH

Material Data Center offers the following functions for KEBAFLOW LCP HF140:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kebaflow datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
成形収縮率, 平行 0.2 % ISO 294-4, 2577
成形収縮率, 直角 0.5 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 15000 MPa ISO 527
破壊応力 140 MPa ISO 527
破壊ひずみ 1.5 % ISO 527
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 308 °C ISO 75-1/-2
厚さhでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 0.8 mm -
電気的特性.単位テスト基準
ISO データ
体積抵抗率 1E13 Ohm*m IEC 62631-3-1
表面抵抗率 1E15 Ohm IEC 62631-3-2
その他の特性.単位テスト基準
吸水率. 0.02 % Sim. to ISO 62
密度. 1680 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 150 - 170 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.01 % -
樹脂温度 335 - 345 °C -
金型温度 80 - 120 °C -
Back pressure 0 - 3 MPa -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
難燃., 熱安定化.
耐薬品性
General Chemical Resistance
アプリケーション
航空宇宙, 自動車, 電気電子, カプセル化された
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com