Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KEYFLEX TO1192A - TPV - LG Chem

Material Data Center offers the following functions for KEYFLEX TO1192A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Keyflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 20 g/10min ASTM D 1238
温度 230 °C -
荷重 10 kg -
機械的特性単位テスト基準
ASTM数据
破壊応力 9.81 MPa ASTM D 638
破断伸び 700 % ASTM D 638
ショア硬さA 92 - ASTM D 2240
引裂強さ 54 kN/m ASTM D 624
ノッチ付きIzod衝撃強さ, 1/4 in N J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature N J/m ASTM D 256
温度 -40 °C -
その他の特性.単位テスト基準
密度 930 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 60 - 90 °C -
Pre-drying - Time 3 - 4 h -
樹脂温度 200 - 240 °C -
金型温度 40 - 60 °C -
Zone 1 180 - 200 °C -
Zone 2 180 - 220 °C -
Zone 3 200 - 230 °C -
Screw speed 30 - 60 rpm -
Back pressure 30 - 60 MPa -
特殊な特性
成形加工法.
カレンダー加工.
な特性
Soft Feel
アプリケーション
自動車, 汎用
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.