Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kocetal® GF305 - POM-GF25 - Kolon Industries

Material Data Center offers the following functions for Kocetal® GF305:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kocetal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 7 g/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
成形収縮率, 平行 0.8 % ISO 294-4, 2577
成形収縮率, 直角 1.4 % ISO 294-4, 2577
ASTM数据
メルトフローレイト, MFI 7 g/10min ASTM D 1238
温度 190 °C -
荷重 2.16 kg -
成形収縮率., 平行 0.005 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張強度 130 MPa ISO 527
破壊ひずみ 4 % ISO 527
曲げ弾性率, 23°C 8500 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 7 kJ/m² ISO 179/1eA
ロックウェル硬度 M 96 - ISO 2039-2
ASTM数据
引張強度 128 MPa ASTM D 638
破断伸び 6 % ASTM D 638
曲げ弾性率 8000 MPa ASTM D 790
曲げ強さ 190 MPa ASTM D 790
ロックウェル硬度 M 90 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 50 J/m ASTM D 256
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 166 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 161 °C ISO 75-1/-2
ASTM数据
UL94 燃焼性 HB - UL 94
追加試験片の厚さ 0.8 mm -
線膨張係数, 平行 25 E-6/K ASTM D 696
DTUL @ 66 psi 164 °C ASTM D 648
DTUL @ 264 psi 163 °C ASTM D 648
溶融温度 166 °C ASTM D 3418
電気的特性.単位テスト基準
ISO データ
体積抵抗率 1E12 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
耐電圧 19 kV/mm IEC 60243-1
ASTM数据
耐電圧, 短い時間 19 kV/mm ASTM D 149
誘電正接, 1 MHz 0.006 - ASTM D 150
表面抵抗率 >1E15 Ohm ASTM D 257
体積抵抗率 1E14 Ohm*cm ASTM D 257
その他の特性.単位テスト基準
密度. 1590 kg/m³ ISO 1183
吸水率, 24hr 0.2 % ASTM D 570
密度 1590 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 3 h -
樹脂温度 ≤220 °C -
金型温度 70 - 120 °C -
Zone 1 180 °C -
Zone 2 200 °C -
Zone 3 200 °C -
Nozzle temperature 210 °C -
特殊な特性
成形加工法.
射出成形.
領域別の利用可能性
北アメリカ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.