Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KDCL1050 - PA66-CF50 - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KDCL1050:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
成形収縮率, 平行 0.2 % ISO 294-4, 2577
ASTM数据
成形収縮率., 平行 0.002 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張強度 345 MPa ISO 527
曲げ弾性率 33500 MPa ISO 178
曲げ強さ 510 MPa ISO 178
シャルピー衝撃強さ, +23°C 75 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 24 kJ/m² ISO 179/1eA
ロックウェル硬度 R 122 - ISO 2039-2
ASTM数据
引張弾性率 41300 MPa ASTM D 638
引張強度 330 MPa ASTM D 638
曲げ弾性率 35800 MPa ASTM D 790
曲げ強さ 510 MPa ASTM D 790
ロックウェル硬度 R 122 - ASTM D 785
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 262 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 255 °C ISO 75-1/-2
ASTM数据
UL94 燃焼性 HB - UL 94
DTUL @ 264 psi 255 °C ASTM D 648
溶融温度 262 °C ASTM D 3418
その他の特性.単位テスト基準
密度. 1370 kg/m³ ISO 1183
吸水率, 24hr 0.5 % ASTM D 570
密度 1370 kg/m³ ASTM D 792
特殊な特性
特殊な特性.
高耐衝撃及び耐衝撃改良.
な特性
Creep Resistance
アプリケーション
自動車, 電気電子
領域別の利用可能性
北アメリカ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.