Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar Flex® 2751-00 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar Flex® 2751-00:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Kynar Flex® resins are fluorinated thermoplastic copolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, barrier properties and high purity.

Kynar Flex® 2751-00 resin is a powder grade where maximum flexibility or impact strength is required.


Main applications:
  • flexible tubing
  • corrosion protection in the chemical industry
  • off-shore
  • wire and cable
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 1.9 cm³/10min ISO 1133
温度 230 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 450 MPa ISO 527
降伏応力 21 MPa ISO 527
降伏ひずみ 15 % ISO 527
破壊呼びひずみ >50 % ISO 527
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 134 °C ISO 11357-1/-3
ガラス転移点, 10°C/min -40 °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 40 °C ISO 75-1/-2
厚さhでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 0.8 mm -
酸素指数 43 % ISO 4589-1/-2
電気的特性.単位テスト基準
ISO データ
体積抵抗率 2E12 Ohm*m IEC 62631-3-1
特殊な特性
納入形状.
パウダー.
な特性
Copolymer
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.