Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar® UHM 6020-20 - PVDF-GF - ARKEMA

Material Data Center offers the following functions for Kynar® UHM 6020-20:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Kynar® resins are fluorinated thermoplastic homopolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, high barrier properties, high purity, excellent mechanical and thermo-mechanical properties.

Kynar® UHM 6020-20 resin is a specific grade of granules for injection, extrusion, compression and transfer molding. 

This grade has specific improved mechanical properties where extreme conditions in temperature and pressure are needed.


Main applications:
  • corrosion protection in the chemical industry

機械的特性単位テスト基準
ISO データ
引張弾性率 7900 MPa ISO 527
破壊応力 120 MPa ISO 527
破壊ひずみ 3 % ISO 527
引張クリープ弾性率, 1h 7900 MPa ISO 899-1
引張クリープ弾性率, 1000h 7900 MPa ISO 899-1
シャルピー衝撃強さ, +23°C 44 kJ/m² ISO 179/1eU
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 170 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 159 °C ISO 75-1/-2
線膨張係数, 平行 35 E-6/K ISO 11359-1/-2
線膨張係数, 直角 35 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 V-0 class IEC 60695-11-10
その他の特性.単位テスト基準
吸水率 0 % Sim. to ISO 62
吸湿率 0 % Sim. to ISO 62
特殊な特性
成形加工法.
射出成形., 異形押出成形., トランスファー成形.
納入形状.
ペレット.
な特性
Homopolymer
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.