Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LIM® 6050 - VMQ - Momentive Performance Materials Inc.

Material Data Center offers the following functions for LIM® 6050:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other LIM datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Appearance/Color:
liquid, transparent

Characteristics:
fast cure, high tear strength

Conformity:
The product meets the requirements for passing the test standards USP Class VI, FDA 21 CFR 177.2600 and ISO 10993.
Based on listing of ingredients in the BfR recommendation XV "Silicones", the product is compositionally compliant.

These values were determined with the following conditions:
Postbaked 1 hr @ 204ºC / 400ºF.

Other values were achieved with the following conditions:
As Molded 30 sec @ 177ºC / 350ºF:


Property Value Unit Standard
Shore A hardness, 3s 50 - ISO 868
Tensile Strength 8.6 MPa
ISO 37
Strain at break 575 %
ISO 37
Tear Strength 43,9 kN/m
ASTM D 624
機械的特性単位テスト基準
ISO データ
引張強度 9 MPa ISO 37
破壊ひずみ 530 % ISO 37
ショア硬さA 53 - ISO 7619-1
ASTM数据
引裂強さ 43 kN/m ASTM D 624
熱的特性単位テスト基準
ISO データ
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
Yellow Card 可用 はい - -
その他の特性.単位テスト基準
密度. 1120 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
特殊な特性.
透明.
Certifications
Food contact, Food approval BfR, Food approval FDA 21 CFR, US Pharmacopeia Class VI Approved
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.