Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY EU5001 - (PC+ASA) - LG Chem

Material Data Center offers the following functions for LUPOY EU5001:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 21 g/10min ISO 1133
温度 260 °C -
荷重 5 kg -
成形収縮率, 平行 0 % ISO 294-4, 2577
成形収縮率, 直角 0 % ISO 294-4, 2577
ASTM数据
メルトフローレイト, MFI 3 g/10min ASTM D 1238
温度 250 °C -
荷重 2.16 kg -
成形収縮率., 平行 0.007 mm/mm ASTM D 955
成形収縮率, 直角 0.007 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2010 MPa ISO 527
降伏応力 53 MPa ISO 527
降伏ひずみ 5.7 % ISO 527
破壊応力 56 MPa ISO 527
破壊ひずみ 100 % ISO 527
曲げ弾性率, 23°C 2120 MPa ISO 178
曲げ強さ 82 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 60[1] kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30゚C 15[1] kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C 56[1] kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 16[1] kJ/m² ISO 180/1A
温度 -30 °C -
ロックウェル硬度 R 115 - ISO 2039-2
ASTM数据
引張弾性率 1981 MPa ASTM D 638
降伏応力 54 MPa ASTM D 638
破壊応力 62.8 MPa ASTM D 638
降伏点伸び 5.8 % ASTM D 638
破断伸び 116 % ASTM D 638
曲げ弾性率 2040 MPa ASTM D 790
曲げ強さ 90.3 MPa ASTM D 790
ロックウェル硬度 R 115 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 677 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, 1/4 in 540 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 147 J/m ASTM D 256
温度 -30 °C -
1: 4 mm
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 106[2] °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 130[2] °C ISO 75-1/-2
ビカット軟化温度, B 133 °C ISO 306
線膨張係数, 平行 89 E-6/K ISO 11359-1/-2
線膨張係数, 直角 92 E-6/K ISO 11359-1/-2
ASTM数据
線膨張係数, 平行 89 E-6/K ASTM D 696
線膨張係数, 直角 92 E-6/K ASTM D 696
DTUL @ 66 psi 132 °C ASTM D 648
DTUL @ 264 psi 115 °C ASTM D 648
ビカット軟化温度 134 °C ASTM D 1525
2: 4 mm
電気的特性.単位テスト基準
ISO データ
体積抵抗率 1E15 Ohm*m IEC 62631-3-1
表面抵抗率 1E15 Ohm IEC 62631-3-2
ASTM数据
耐電圧, 短い時間 19 kV/mm ASTM D 149
表面抵抗率 1E15 Ohm ASTM D 257
体積抵抗率 1E17 Ohm*cm ASTM D 257
その他の特性.単位テスト基準
吸湿率 0.2 % Sim. to ISO 62
密度. 1160 kg/m³ ISO 1183
密度 1160 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 - 100 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
樹脂温度 240 - 270 °C -
金型温度 60 - 80 °C -
Zone 1 240 - 260 °C -
Zone 2 240 - 260 °C -
Zone 3 245 - 265 °C -
Nozzle temperature 245 - 260 °C -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
紫外線安定化.
アプリケーション
電気電子, 汎用
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.