Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® ECO 358N BC70 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® ECO 358N BC70:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Luran® ECO 358N BC70 is the general purpose easy-flow grade of SAN, suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very good transparency and a light intrinsic color. Luran® ECO 358N BC70 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 93 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 70 %
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 22 cm³/10min ISO 1133
温度 220 °C -
荷重 10 kg -
成形収縮率, 平行 0.5 % ISO 294-4, 2577
溶融時の熱伝導率 0.17 W/(m K) -
機械的特性単位テスト基準
ISO データ
引張弾性率 3700 MPa ISO 527
破壊応力 72 MPa ISO 527
破壊ひずみ 3 % ISO 527
曲げ弾性率, 23°C 3600 MPa ISO 178
曲げ強さ 120 MPa ISO 178
シャルピー衝撃強さ, +23°C 16 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 16 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 2 kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C 2 kJ/m² ISO 180/1A
Ball indentation hardness 165 MPa ISO 2039-1
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 86 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 99 °C ISO 75-1/-2
ビカット軟化温度, B 106 °C ISO 306
線膨張係数, 平行 70 E-6/K ISO 11359-1/-2
Other Standards[S]
熱伝導率, ソリッド 0.17 W/(m K) DIN 52612-1
S: These properties are reported by the producer according standards that are different to our defaults.
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 3 - IEC 62631-2-1
誘電正接, 100Hz 40 E-4 IEC 62631-2-1
誘電正接, 1MHz 70 E-4 IEC 62631-2-1
体積抵抗率 1E14 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
光学特性単位テスト基準
Other Standards[S]
くっせつりつ 1.57 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
吸湿率 0.2 % Sim. to ISO 62
密度 1080 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 220 - 260 °C -
金型温度 40 - 80 °C -
Injection speed 200 mm/s -
機能
 粘度せん断速度. , Luran® ECO 358N BC70, SAN, INEOS Styrolution
 せん断応力-せん断速度. , Luran® ECO 358N BC70, SAN, INEOS Styrolution
 応力-ひずみ. , Luran® ECO 358N BC70, SAN, INEOS Styrolution
 割線弾性率−ひずみ. , Luran® ECO 358N BC70, SAN, INEOS Styrolution
 応力-ひずみ (等時的). 23°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 クリープ弾性率−時間. 23°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
クリープ曲線 23°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 応力-ひずみ (等時的). 40°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 クリープ弾性率−時間. 40°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
クリープ曲線 40°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 応力-ひずみ (等時的). 60°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 クリープ弾性率−時間. 60°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
クリープ曲線 60°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 応力-ひずみ (等時的). 80°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 クリープ弾性率−時間. 80°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
クリープ曲線 80°C, Luran® ECO 358N BC70, SAN, INEOS Styrolution
 pvT , Luran® ECO 358N BC70, SAN, INEOS Styrolution
 引張弾性率-温度. , Luran® ECO 358N BC70, SAN, INEOS Styrolution
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
熱安定化., 透明.
耐薬品性
General Chemical Resistance
Certifications
Contains renewable resources, Food contact, ISCC Plus
アプリケーション
汎用, パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 近東/アフリカ
その他の情報
村遜速揃
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 260°C

Mold temperature, range: 40 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com