Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® 1248 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® 1248 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Partially bio-circular grade.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 7 cm³/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
メルトフローレート, MFI 7.5 g/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
成形収縮率, 平行 0.8 % ISO 294-4, 2577
成形収縮率, 直角 0.8 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 2250 MPa ISO 527
降伏応力 61 MPa ISO 527
降伏ひずみ 6 % ISO 527
破壊呼びひずみ >50 % ISO 527
破壊応力 70 MPa ISO 527
破壊ひずみ 130 % ISO 527
曲げ弾性率, 23°C 2250 MPa ISO 178
曲げ強さ 88 MPa ISO 178
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30゚C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C, 3mm 70 kJ/m² ISO 179/1eA
Type of failure P - -
ノッチ付きシャルピー衝撃強さ, -30°C, 3mm 60 kJ/m² ISO 179/1eA
Type of failure P(C) - -
ノッチ付きIzod衝撃強さ, +23°C 65 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 30 kJ/m² ISO 180/1A
温度 -30 °C -
パンクチャー衝撃-最大応力, +23゚C 5200 N ISO 6603-2
パンクチャー衝撃-最大応力, -30゚C 6100 N ISO 6603-2
パンクチャー衝撃エネルギー, +23゚C 55 J ISO 6603-2
パンクチャー衝撃エネルギー, -30゚C 60 J ISO 6603-2
Ball indentation hardness 108 MPa ISO 2039-1
熱的特性単位テスト基準
ISO データ
ガラス転移点, 10゚C/min 148 °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 125 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 139 °C ISO 75-1/-2
ビカット軟化温度, B 146 °C ISO 306
線膨張係数, 平行 70 E-6/K ISO 11359-1/-2
線膨張係数, 直角 70 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
酸素指数 30 % ISO 4589-1/-2
グローワイヤ燃焼性指数 (GWFI) 850 °C IEC 60695-2-12
GWFI - 試験片の厚さ 0.75 mm -
グローワイヤ燃焼性指数 (GWFI) 850 °C IEC 60695-2-12
GWFI - 試験片の厚さ 1.5 mm -
グローワイヤ燃焼性指数 (GWFI) 900 °C IEC 60695-2-12
GWFI - 試験片の厚さ 3 mm -
グローワイヤ着火温度 (GWIT) 800 °C IEC 60695-2-13
GWIT - 試験片の厚さ 0.75 mm -
グローワイヤ着火温度 (GWIT) 875 °C IEC 60695-2-13
GWIT - 試験片の厚さ 1.5 mm -
グローワイヤ着火温度 (GWIT) 875 °C IEC 60695-2-13
GWIT - 試験片の厚さ 3 mm -
Other Standards[S]
熱伝導率, ソリッド 0.2 W/(m K) ISO 8302
S: These properties are reported by the producer according standards that are different to our defaults.
電気的特性.単位テスト基準
ISO データ
体積抵抗率 1E14 Ohm*m IEC 62631-3-1
表面抵抗率 1E16 Ohm IEC 62631-3-2
耐電圧 34 kV/mm IEC 60243-1
耐トラッキング性 225 - IEC 60112
Other Standards[S]
比誘電率, 100Hz 3.1 - IEC 60250
比誘電率, 1MHz 3 - IEC 60250
誘電正接, 100Hz 12 E-4 IEC 60250
誘電正接, 1MHz 120 E-4 IEC 60250
S: These properties are reported by the producer according standards that are different to our defaults.
光学特性単位テスト基準
ISO Data
視感透過率 89[1] % ISO 13468-1, -2
Other Standards[S]
くっせつりつ 1.59 - ISO 489
1: 2 mm  S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
吸水率. 0.4 % Sim. to ISO 62
吸湿率 0.12 % Sim. to ISO 62
密度. 1200 kg/m³ ISO 1183
Bulk density 640 kg/m³ -
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 300 °C ISO 294
射出成形, 金型温度 80 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 120 °C -
Pre-drying - Time 2 - 3 h -
Processing humidity ≤0.02 % -
樹脂温度 280 - 320 °C -
金型温度 80 - 120 °C -
Zone 1 250 - 260 °C -
Zone 2 270 - 280 °C -
Zone 3 280 - 290 °C -
Nozzle temperature 290 - 300 °C -
Back pressure 5 - 15 MPa -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
高耐衝撃及び耐衝撃改良.
Certifications
Contains renewable resources, Food contact, ISCC Plus
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.