Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Naturacell® - CA - Rotuba

Material Data Center offers the following functions for Naturacell®:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Naturacell datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
For more detailed information, please read our
or contact our representatives in your region.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 0.25 g/10min ASTM D 1238
成形収縮率., 平行 0.0007 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
降伏応力 23.5 MPa ASTM D 638
破壊応力 22.4 MPa ASTM D 638
破断伸び 13 % ASTM D 638
曲げ弾性率 1034 MPa ASTM D 790
ロックウェル硬度 R29 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 107 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 16 J/m ASTM D 256
温度 -40 °C -
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 63.9 °C ASTM D 648
DTUL @ 264 psi 53.9 °C ASTM D 648
ビカット軟化温度 87.2 °C ASTM D 1525
光学特性単位テスト基準
ASTM数据
ヘイズ 0.88 % ASTM D 1003
視感透過率 90 % ASTM D 1003
その他の特性.単位テスト基準
吸水率, 24hr 7.7 % ASTM D 570
密度 1290 kg/m³ ASTM D 792
特殊な特性
納入形状.
ペレット.
特殊な特性.
透明.
耐薬品性
General Chemical Resistance
Certifications
Contains renewable resources
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.