Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIPLENE F30 AGR HF - PP-GF30 - Soredi S.p.a.

Material Data Center offers the following functions for NIPLENE F30 AGR HF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 10 g/10min ASTM D 1238
温度 230 °C -
荷重 2.16 kg -
成形収縮率., 平行 0.004 mm/mm ASTM D 955
成形収縮率, 直角 0.006 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
破壊応力 90 MPa ASTM D 638
曲げ弾性率 6000 MPa ASTM D 790
曲げ強さ 140 MPa ASTM D 790
ロックウェル硬度 R 113 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 125 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 76.9 J/m ASTM D 256
温度 -20 °C -
熱的特性単位テスト基準
ISO データ
線膨張係数, 直角 30 E-6/K ISO 11359-1/-2
ASTM数据
UL94 燃焼性 HB - UL 94
追加試験片の厚さ 1.6 mm -
DTUL @ 264 psi 153 °C ASTM D 648
ビカット軟化温度 144 °C ASTM D 1525
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 2.7 - IEC 62631-2-1
体積抵抗率 1E13 Ohm*m IEC 62631-3-1
表面抵抗率 1E14 Ohm IEC 62631-3-2
耐電圧 60 kV/mm IEC 60243-1
その他の特性.単位テスト基準
吸湿率 0.1 % Sim. to ISO 62
密度 1120 kg/m³ ASTM D 792
特殊な特性
な特性
Chemically Coupled Reinforcement, Homopolymer
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.