Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NOVADURAN 5510S - PBT - Mitsubishi Engineering-Plastics Corporation

Material Data Center offers the following functions for NOVADURAN 5510S:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Novaduran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 33 cm³/10min ISO 1133
温度 250 °C -
荷重 2.16 kg -
成形収縮率, 平行 2.2 % ISO 294-4, 2577
成形収縮率, 直角 2.0 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 420 MPa ISO 527
降伏応力 21 MPa ISO 527
降伏ひずみ 21 % ISO 527
破壊ひずみ 200 % ISO 527
曲げ弾性率, 23°C 360 MPa ISO 178
曲げ強さ 22 MPa ISO 178
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 30 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 219 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 74 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 139 °C ISO 75-1/-2
線膨張係数, 平行 150 E-6/K ISO 11359-1/-2
線膨張係数, 直角 150 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
Yellow Card 可用 はい - -
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 3.2 - IEC 62631-2-1
誘電正接, 1MHz 200 E-4 IEC 62631-2-1
体積抵抗率 1E14 Ohm*m IEC 62631-3-1
表面抵抗率 1E15 Ohm IEC 62631-3-2
耐電圧 22 kV/mm IEC 60243-1
その他の特性.単位テスト基準
吸水率. 0.4 % Sim. to ISO 62
密度. 1240 kg/m³ ISO 1183
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 120 °C -
Pre-drying - Time 5 - 8 h -
金型温度 60 - 100 °C -
Zone 1 240 - 260 °C -
Zone 2 240 - 260 °C -
Zone 3 240 - 260 °C -
Nozzle temperature 260 °C -
特殊な特性
成形加工法.
その他の押出成形.
な特性
Copolymer, Impact Copolymer
アプリケーション
自動車, 電気電子, 汎用
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.