Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® E3TZ - ABS - INEOS Styrolution

Material Data Center offers the following functions for Novodur® E3TZ:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Novodur® E3TZ acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® E3TZ is an extrusion grade with high gloss and good surface appearance. It is optimized for processing via thermoforming. Furthermore, food contact statements are available upon request.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 8 cm³/10min ISO 1133
温度 220 °C -
荷重 10 kg -
成形収縮率, 平行 0.6 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 2550 MPa ISO 527
降伏応力 48 MPa ISO 527
降伏ひずみ 2.5 % ISO 527
破壊呼びひずみ 15 % ISO 527
曲げ弾性率, 23°C 2600 MPa ISO 178
曲げ強さ 75 MPa ISO 178
シャルピー衝撃強さ, +23°C 150 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 110 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 19 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 9 kJ/m² ISO 179/1eA
Ball indentation hardness 110 MPa ISO 2039-1
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 98 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 103 °C ISO 75-1/-2
ビカット軟化温度, B 100 °C ISO 306
線膨張係数, 平行 90 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
グローワイヤ燃焼性指数 (GWFI) 700 °C IEC 60695-2-12
GWFI - 試験片の厚さ 2 mm -
電気的特性.単位テスト基準
ISO データ
表面抵抗率 600 Ohm IEC 62631-3-2
耐電圧 35 kV/mm IEC 60243-1
その他の特性.単位テスト基準
密度 1050 kg/m³ ISO 1183
Processing Recommendation Extrusion単位テスト基準
Type of extrusion profile - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 215 - 240 °C -
Type of extrusion sheet - -
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 215 - 240 °C -
特殊な特性
成形加工法.
異形押出成形., シート押出成形., その他の押出成形., 熱成形.
納入形状.
ペレット.
特殊な特性.
高耐衝撃及び耐衝撃改良.
な特性
High Gloss
Certifications
Food contact
領域別の利用可能性
ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
その他の情報
族臓遜造揃
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Profiles, Melt temperature: 215 - 240°C

促揃臓村促速揃
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Sheets, Melt temperature: 215 - 240°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.