Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® Ultra 4255 - (ABS+PC) - INEOS Styrolution

Material Data Center offers the following functions for Novodur® Ultra 4255:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Novodur® Ultra 4255 acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® Ultra 4255 is PC modified injection molding grade combining very high impact strength at room as well as at low temperature, 100 % ductility at -30 °C, high heat resistance and a best in class flowability. Furthermore, it is of low emission, i.e. suitable to produce parts which fulfill interior emission requirements of the automotive OEMs.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 17 cm³/10min ISO 1133
温度 260 °C -
荷重 5 kg -
溶融時の密度 966 kg/m³ -
溶融時の熱伝導率 0.211 W/(m K) -
溶融時の比熱 2250 J/(kg K) -
突き出し時の時の温度 101 °C -
機械的特性単位テスト基準
ISO データ
引張弾性率 2100 MPa ISO 527
降伏応力 47 MPa ISO 527
降伏ひずみ 4.1 % ISO 527
破壊呼びひずみ >50 % ISO 527
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 55 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 55 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 103 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 116 °C ISO 75-1/-2
ビカット軟化温度, B 110 °C ISO 306
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
Yellow Card 可用 はい - -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 3.0 mm -
Yellow Card 可用 はい - -
電気的特性.単位テスト基準
ISO データ
耐電圧 35 kV/mm IEC 60243-1
耐トラッキング性 275 - IEC 60112
その他の特性.単位テスト基準
密度 1100 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
な特性
Low Emission
領域別の利用可能性
北アメリカ., ヨーロッパ., 南・中央アメリカ., 近東/アフリカ
その他の情報
村遜速揃
PREPROCESSING

Pre-drying, Temperature: 80 - 90°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 250 - 270°C

Mold temperature, range: 60 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.