Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PHARMALENE® MT 10 PH BCA - (PE-LD) - Versalis S.p.A

Material Data Center offers the following functions for PHARMALENE® MT 10 PH BCA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pharmalene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Pharmalene MT 10 PH BCA will be bio attributed for 100%.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 40 g/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
降伏応力 9 MPa ISO 527
曲げ弾性率, 23°C 110 MPa ISO 178
ショア硬さD 43 - ISO 7619-1
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 106 °C ISO 11357-1/-3
ビカット軟化温度, A 80 °C ISO 306
その他の特性.単位テスト基準
密度. 917 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
金型温度 10 - 30 °C -
Zone 1 160 - 200 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
Certifications
Contains renewable resources, Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Medical Grade, US Pharmacopeia Class VI Approved, ISCC Plus
アプリケーション
医療の
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.