Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® H 2528 Powder - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® H 2528 Powder:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Platamid® H 2528 Powder
Copolyamide Hot Melt Adhesive / Textile Applications

Platamid® H 2528 Powder is a medium melt viscosity copolyamide adhesive powder for the production of fusible interlinings.
Platamid® H 2528 Powder offers excellent laundry resistance up to 60°C and an excellent steam resistance at moderate fusing conditions.  

AVAILABLE GRADES

This grade is available in different grain sizes:

- Platamid® H 2528 PA80 (0-80 µm paste dot)

- Platamid® H 2528 PTA 120 (0-120 µm power dot)

- Platamid® H 2528 PTA 170/20 (0-170 µm power dot)

- Platamid® H 2528 PTA 170 (80-170 µm double dot)

PACKAGING
Platamid® H 2528 PTA 170, Platamid® H 2528 PA80, Platamid® H 2528 PTA 120 and Platamid® H 2528 PTA 170/20 are delivered in 20 kg sealed bags. 
SHELF LIFE

Two years from the date of delivery. For any use above this limit, please refer to our technical services.

 

Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 44 / * cm³/10min ISO 1133
温度 160 / * °C -
荷重 2.16 / * kg -
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 128 / * °C ISO 11357-1/-3
特殊な特性
納入形状.
パウダー.
な特性
Copolymer
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.