Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® Clear G850 Rnew® - PA* - ARKEMA

Material Data Center offers the following functions for Rilsan® Clear G850 Rnew®:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
PA,,GHT,C14-020

Rilsan® Clear G850 Rnew® is a high performance transparent copolyamide, partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited for optic as high end eyewear frames.

According to ASTM D6866, the biobased carbon content is measured at 45%.



Main applications:
  • Sun
  • optical
  • reading glass frames
  • Structural frames of smart phones
  • Watch covers
  • Household appliances

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit,  please refer to our technical services.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 4.4 / * cm³/10min ISO 1133
温度 275 / * °C -
荷重 2.16 / * kg -
成形収縮率, 平行 0.9 / * % ISO 294-4, 2577
成形収縮率, 直角 0.9 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 1680 / 1640 MPa ISO 527
降伏応力 64 / 58 MPa ISO 527
降伏ひずみ 8.2 / 8.6 % ISO 527
破壊呼びひずみ >50 / >50 % ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 8.5 / 15 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 8.6 / 11.4 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
ガラス転移点, 10°C/min 145 / * °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 120 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 135 / * °C ISO 75-1/-2
1.5mm厚さでの燃焼性 V-2 / * class IEC 60695-11-10
試験片の厚さ 1.6 / * mm -
Yellow Card 可用 はい / * - -
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm -
Yellow Card 可用 はい / * - -
その他の特性.乾燥/調湿単位テスト基準
吸水率 4 / * % Sim. to ISO 62
吸湿率 1.7 / * % Sim. to ISO 62
密度 1010 / 1010 kg/m³ ISO 1183
Biobased content 45 % -
機能
 粘度せん断速度. , Rilsan® Clear G850 Rnew®, PA*, ARKEMA
 せん断応力-せん断速度. , Rilsan® Clear G850 Rnew®, PA*, ARKEMA
 pvT , Rilsan® Clear G850 Rnew®, PA*, ARKEMA
特殊な特性
成形加工法.
射出成形., フィルム押出成形.
納入形状.
ペレット.
特殊な特性.
熱安定化., 透明.
Certifications
Contains renewable resources
領域別の利用可能性
その他の情報
村遜速揃
Injection Process conditions:
- Typical melt temperature  (Min / Recommended / Max)  : 250°C / 280°C / 300°C
- Typical mold temperature  : 20 - 80 °C
- Dyring time and temperature (only for bags opened for more than two hours): 4 - 6 hours at 90°C
フィルム押出成形.
Extrusion Process conditions:
- Typical melt temperature  (Min / Recommended / Max)  : 250°C / 270°C / 290°C
- Dyring time and temperature (only for bags opened for more than two hours): 4 - 6 hours at 90°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.