Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SKYPEL G172D - TPE - SK Chemicals

Material Data Center offers the following functions for SKYPEL G172D:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Skypel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 13 g/10min ASTM D 1238
温度 230 °C -
荷重 2.16 kg -
成形収縮率., 平行 0.017 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
破壊応力 46 MPa ASTM D 638
破断伸び 420 % ASTM D 638
曲げ弾性率 540 MPa ASTM D 790
ショア硬さD 72 - ASTM D 2240
ノッチ付きIzod衝撃強さ, 1/4 in 120 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 150 °C ASTM D 648
溶融温度 218 °C ASTM D 3418
その他の特性.単位テスト基準
吸水率, 24hr 0.3 % ASTM D 570
密度 1250 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 100 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.1 % -
金型温度 40 °C -
Zone 1 220 °C -
Zone 2 230 °C -
Zone 3 230 °C -
Nozzle temperature 235 °C -
特殊な特性
成形加工法.
射出成形., その他の押出成形.
特殊な特性.
高耐衝撃及び耐衝撃改良., 紫外線安定化., 熱安定化.
な特性
Creep Resistance, Cut Through Resistance, Fatigue Resistance, Copolymer
耐薬品性
General Chemical Resistance, Solvent Resistance, Oil Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.