Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Spectar™ - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Spectar™:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Spectar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastman Spectar™ Clear is a copolyester, developed by Eastman to achieve measurably improved sheet clarity and edge color while maintaining the performance characteristics for which Eastman Spectar™ copolyester has become known in the industry. It offers the thermoformability and ease of fabrication of Eastman Spectar™ copolyester along with significantly improved clarity. Eastman Spectar™ Clear also offers approximately double the notch impact strength, 50% higher instrumented impact strength and better chemical resistance when compared

to traditional Spectar™ Copolyester.




機械的特性単位テスト基準
ASTM数据
引張弾性率 1800 MPa ASTM D 638
降伏応力 48 MPa ASTM D 638
破壊応力 53 MPa ASTM D 638
降伏点伸び 5 % ASTM D 638
破断伸び 340 % ASTM D 638
曲げ弾性率 2000 MPa ASTM D 790
ロックウェル硬度 R 107 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in N J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 83 J/m ASTM D 256
温度 -30 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
UL94 燃焼性 HB - UL 94
線膨張係数, 平行 76.2 E-6/K ASTM D 696
DTUL @ 66 psi 77 °C ASTM D 648
DTUL @ 264 psi 73 °C ASTM D 648
ビカット軟化温度 86 °C ASTM D 1525
電気的特性.単位テスト基準
ASTM数据
表面抵抗率 1E17 Ohm ASTM D 257
体積抵抗率 1E16 Ohm*cm ASTM D 257
耐アーク 130 s ASTM D 495
光学特性単位テスト基準
ASTM数据
光沢度 150 - ASTM D 2457
ヘイズ 0.5 % ASTM D 1003
視感透過率 91 % ASTM D 1003
その他の特性.単位テスト基準
吸水率, 24hr 0.19 % ASTM D 570
密度 1230 kg/m³ ASTM D 792
特殊な特性
成形加工法.
シート押出成形., 熱成形.
特殊な特性.
高耐衝撃及び耐衝撃改良., 透明.
な特性
Low Odor, Copolymer
耐薬品性
General Chemical Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.