Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Stylac NF920 - ACS - Asahi Kasei

Material Data Center offers the following functions for Stylac NF920:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Stylac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 55 cm³/10min ISO 1133
温度 220 °C -
荷重 10 kg -
メルトフローレート, MFI 59 g/10min ISO 1133
温度 220 °C -
荷重 10 kg -
ASTM数据
成形収縮率., 平行 0.0055 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
降伏応力 44 MPa ISO 527
曲げ弾性率, 23°C 2550 MPa ISO 178
曲げ強さ 70 MPa ISO 178
ノッチ付きシャルピー衝撃強さ, +23°C 7 kJ/m² ISO 179/1eA
ロックウェル硬度 R 101 - ISO 2039-2
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 74 °C ISO 75-1/-2
ビカット軟化温度, B 88 °C ISO 306
厚さhでの燃焼性 5V 5VA class IEC 60695-11-20
試験片の厚さ 2.5 mm -
ASTM数据
UL94 燃焼性 V-0 - UL 94
追加試験片の厚さ 1.5 mm -
線膨張係数, 平行 85 E-6/K ASTM D 696
その他の特性.単位テスト基準
密度. 1160 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 70 - 80 °C -
Pre-drying - Time 3 - 4 h -
金型温度 40 - 50 °C -
Zone 1 150 - 180 °C -
Zone 2 150 - 190 °C -
Zone 3 170 - 200 °C -
Nozzle temperature 170 - 200 °C -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
難燃.
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.