Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TPX® DX231 - PMP - Mitsui Chemicals America, Inc.

Material Data Center offers the following functions for TPX® DX231:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other TPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 100 g/10min ASTM D 1238
温度 260 °C -
荷重 5 kg -
機械的特性単位テスト基準
ASTM数据
引張弾性率 1862 MPa ASTM D 638
引張強度 25 MPa ASTM D 638
降伏応力 29 MPa ASTM D 638
破断伸び 14 % ASTM D 638
曲げ弾性率 1551 MPa ASTM D 790
曲げ強さ 43 MPa ASTM D 790
ロックウェル硬度 R91 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 18.1 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
線膨張係数, 平行 380 E-6/K ASTM D 696
DTUL @ 66 psi 126 °C ASTM D 648
ビカット軟化温度 180 °C ASTM D 1525
電気的特性.単位テスト基準
ASTM数据
体積抵抗率 1E16 Ohm*cm ASTM D 257
光学特性単位テスト基準
ASTM数据
ヘイズ 2.1 % ASTM D 1003
視感透過率 93 % ASTM D 1003
くっせつりつ 1.46 - ASTM D 542
その他の特性.単位テスト基準
密度 833 kg/m³ ASTM D 792
特殊な特性
成形加工法.
Fiber Extrusion, その他の押出成形.
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.