Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Technyl Star - PA6 - DOMO Engineering Plastics

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Technyl Star" in Material Data Center leads to the following information:

Tradename: Technyl Star
Family: PA6
Producer: DOMO Engineering Plastics
45 hits in the material database
7 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
TECHNYL STAR AF 218 V25 BK 21N PA66-GF
TECHNYL STAR AF 218 V30 BK 21N PA66-GF
TECHNYL STAR AF 218 V35 BK 21N PA66-GF
TECHNYL STAR AF 218 V40 BK 21N PA66-GF
TECHNYL STAR AF 218S V35 BK 21N PA66-GF
TECHNYL STAR AF 219 V30 BK PA66-GF
TECHNYL STAR AF 219 V30 BK LT PA66-GF
TECHNYL STAR AF 219 V30 NC PA66-GF
TECHNYL STAR AF 60SX V30 GY 7035 PA66-GF FR(40)
TECHNYL STAR AF 60SX V30 ORANGE 2 PA66-GF FR(40)
TECHNYL STAR AFX 216 V50 GY 2684 PA66-GF
TECHNYL STAR AFX 216 V50 NC PA66-GF
TECHNYL STAR AFX 218 V50 BK 31N PA66-GF
TECHNYL STAR AFX 218 V60 BK 31N PA66-GF
TECHNYL STAR AFX 218 V60 NC PA66-GF
TECHNYL STAR AFX 60G1 V45 GY 2633 PA66-GF FR(40)
TECHNYL STAR S 216 V30 NC PA6-GF
TECHNYL STAR S 216 V35 NC PA6-GF
TECHNYL STAR S 216 V50 BK 21N PA6-GF
TECHNYL STAR S 216L2 V30 BK PA6-GF
TECHNYL STAR S 218 MT40 NC PA6-MD
TECHNYL STAR S 218 MZ20 V10 BK 2N PA6-(MD+GF)
TECHNYL STAR S 218 V30 BK 31N PA6-GF
TECHNYL STAR S 218 V30 NC PA6-GF
TECHNYL STAR S 218 V35 BK 31N PA6-GF
TECHNYL STAR S 218 V35 NC PA6-GF
TECHNYL STAR S 218 V60 BK 21N PA6-GF
TECHNYL STAR S 219 V30 NC PA6-GF
TECHNYL STAR S 219 V30 WT 1128 PA6-GF
TECHNYL STAR S 52G1 MX25 GY 2408 PA6-MD FR(30)
TECHNYL STAR S 60X1 V30 BK 15N PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 GY 2408 CF PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 GY 2530 CF PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 GY 2635 PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 GY R7011 PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 GY R7016 CF PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 GY R7035 CF PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 NC PA6-GF FR(40)
TECHNYL STAR S 60X1 V30 WT 2656LPU PA6-GF FR(40)
TECHNYL STAR S 60X2 V30 BK 1N PA6-GF FR(40)
TECHNYL STAR SX 216 V50 NC PA6-GF
TECHNYL STAR SX 216 V60 NC PA6-GF
TECHNYL STAR SX 218 V50 BK Z PA6-GF
TECHNYL STAR SX 218 V60 BK Z PA6-GF
TECHNYL STAR SX 218 V60 NC PA6-GF

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.