Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Terluran® ECO GP-22 MR50 - ABS - INEOS Styrolution

Material Data Center offers the following functions for Terluran® ECO GP-22 MR50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Terluran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
PCR content 50 %
dark grey
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 19 cm³/10min ISO 1133
温度 220 °C -
荷重 10 kg -
成形収縮率, 平行 0.6 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 2100 MPa ISO 527
降伏応力 35 MPa ISO 527
降伏ひずみ 2.6 % ISO 527
破壊応力 25 MPa ISO 527
破壊ひずみ 8 % ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 18 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30゚C 7 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
ビカット軟化温度, B 95 °C ISO 306
その他の特性.単位テスト基準
密度. 1040 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 220 - 260 °C -
金型温度 30 - 80 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
高耐衝撃及び耐衝撃改良., 熱安定化.
な特性
High Gloss
Certifications
Recycled Resin Content
アプリケーション
電気電子
領域別の利用可能性
北アメリカ., ヨーロッパ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.