Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TROGAMID® CX9710 NC - PAPACM12 - Evonik Operations GmbH

Material Data Center offers the following functions for TROGAMID® CX9710 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Trogamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Medium-viscosity and transparent polyamide for injection molding with release agent

TROGAMID® CX9710 is a medium-viscosity and transparent polyamide for injection molding for the manufacture of parts in the optical industry.

The material absorbs only small amounts of water. Components made from this material therefore show excellent dimensional stability under changing ambient humidity as well as consistent UV-stability and chemical resistance. 

TROGAMID® CX9710 is supplied as spherical pellets in moisture-proof packaging.

Pigmentation may affect values.

For information about processing of TROGAMID®, please follow the general commendations about “Processing of TROGAMID® compounds”. 


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.TROGAMID.COM
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 20 / * cm³/10min ISO 1133
温度 285 / * °C -
荷重 5 / * kg -
成形収縮率, 平行 0.7 / * % ISO 294-4, 2577
成形収縮率, 直角 0.8 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 1400 / - MPa ISO 527
降伏応力 60 / - MPa ISO 527
降伏ひずみ 8 / - % ISO 527
破壊呼びひずみ >50 / - % ISO 527
引張クリープ弾性率, 1h * / 1400 MPa ISO 899-1
引張クリープ弾性率, 1000h * / 700 MPa ISO 899-1
シャルピー衝撃強さ, +23°C N / - kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C N / - kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 11 / 10.5 kJ/m² ISO 179/1eA
Type of failure C / C - -
ノッチ付きシャルピー衝撃強さ, -30°C 13 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
ショア硬さD 81 / * - ISO 7619-1
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 250 / * °C ISO 11357-1/-3
ガラス転移点, 10°C/min 140 / * °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 108 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 122 / * °C ISO 75-1/-2
ビカット軟化温度, B 130 / * °C ISO 306
線膨張係数, 平行 90 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 90 / * E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 1.6 / * mm -
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm -
電気的特性.乾燥/調湿単位テスト基準
ISO データ
比誘電率, 100Hz 3.6 / - - IEC 62631-2-1
比誘電率, 1MHz 3.2 / - - IEC 62631-2-1
誘電正接, 100Hz 120 / - E-4 IEC 62631-2-1
誘電正接, 1MHz 325 / - E-4 IEC 62631-2-1
表面抵抗率 * / 1E13 Ohm IEC 62631-3-2
耐トラッキング性 600 / - - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 3.5 / * % Sim. to ISO 62
吸湿率 1.5 / * % Sim. to ISO 62
密度 1020 / - kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形., フィルム押出成形., 異形押出成形., シート押出成形., その他の押出成形., ブロー成形., 熱成形.
納入形状.
ペレット., ナチュラルカラー
添加剤.
離型剤.
特殊な特性.
光安定化., 紫外線安定化., 透明.
耐薬品性
General Chemical Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.