Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4406 G6 HSP - PBT-GF30 FR - BASF

Material Data Center offers the following functions for Ultradur® B 4406 G6 HSP:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Easy flowing Injection molding grade with 30% glass fibers for parts requiring enhanced fire resistance (eg relay housings, plug-in connector, switch and lamp parts)

Abbreviated designation according to ISO 1043: PBT-GF30 FR(17)
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 12 cm³/10min ISO 1133
温度 275 °C -
荷重 2.16 kg -
成形収縮率, 平行 0.3 % ISO 294-4, 2577
成形収縮率, 直角 1.1 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 11700 MPa ISO 527
破壊応力 140 MPa ISO 527
破壊ひずみ 1.9 % ISO 527
曲げ弾性率, 23°C 11300 MPa ISO 178
シャルピー衝撃強さ, +23°C 50 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 7 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 223 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 205 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 220 °C ISO 75-1/-2
線膨張係数, 平行 22 E-6/K ISO 11359-1/-2
線膨張係数, 直角 108 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 1.6 mm -
Yellow Card 可用 はい - -
厚さhでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 0.4 mm -
Yellow Card 可用 はい - -
電気的特性.単位テスト基準
ISO データ
体積抵抗率 1E13 Ohm*m IEC 62631-3-1
表面抵抗率 1E14 Ohm IEC 62631-3-2
耐電圧 37 kV/mm IEC 60243-1
耐トラッキング性 175 - IEC 60112
その他の特性.単位テスト基準
吸水率 0.4 % Sim. to ISO 62
吸湿率 0.2 % Sim. to ISO 62
密度 1700 kg/m³ ISO 1183
Bulk density 750 kg/m³ -
材料特有の特性単位テスト基準
ISO データ
粘度数 90 cm³/g ISO 307, 1157, 1628
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 270 °C ISO 294
射出成形, 金型温度 80 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 - 120 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.04 % -
樹脂温度 250 - 280 °C -
金型温度 60 - 100 °C -
機能
 粘度せん断速度. , Ultradur® B 4406 G6 HSP, PBT-GF30 FR, BASF
 せん断応力-せん断速度. , Ultradur® B 4406 G6 HSP, PBT-GF30 FR, BASF
特殊な特性
成形加工法.
射出成形.
特殊な特性.
難燃.
アプリケーション
電気電子
領域別の利用可能性
北アメリカ., ヨーロッパ.
その他の情報
村遜速揃
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.