Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 6550 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 6550:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
High viscosity grade for compounding or extrusion of semi-finished products, profiles and pipes or cable sheathing.

The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.

Abbreviated designation according to ISO 1043-1: PBT
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 9 cm³/10min ISO 1133
温度 250 °C -
荷重 2.16 kg -
成形収縮率, 平行 1.7 % ISO 294-4, 2577
成形収縮率, 直角 2.1 % ISO 294-4, 2577
ASTM数据
成形収縮率., 平行 0.015 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2400 MPa ISO 527
降伏応力 54 MPa ISO 527
降伏ひずみ 3.5 % ISO 527
破壊呼びひずみ >50 % ISO 527
引張クリープ弾性率, 1h 1800 MPa ISO 899-1
引張クリープ弾性率, 1000h 1100 MPa ISO 899-1
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 250 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 6 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 3.5 kJ/m² ISO 179/1eA
ASTM数据
引張弾性率 2482 MPa ASTM D 638
降伏応力 60 MPa ASTM D 638
降伏点伸び 3.5 % ASTM D 638
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 223 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 50 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 130 °C ISO 75-1/-2
線膨張係数, 平行 110 E-6/K ISO 11359-1/-2
線膨張係数, 直角 110 E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 1.5 mm -
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 0.8 mm -
ASTM数据
DTUL @ 66 psi 135 °C ASTM D 648
DTUL @ 264 psi 53.9 °C ASTM D 648
溶融温度 223 °C ASTM D 3418
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 3.3 - IEC 62631-2-1
比誘電率, 1MHz 3.3 - IEC 62631-2-1
誘電正接, 100Hz 10 E-4 IEC 62631-2-1
誘電正接, 1MHz 200 E-4 IEC 62631-2-1
体積抵抗率 >1E13 Ohm*m IEC 62631-3-1
表面抵抗率 1E13 Ohm IEC 62631-3-2
耐トラッキング性 600 - IEC 60112
その他の特性.単位テスト基準
吸水率 0.5 % Sim. to ISO 62
吸湿率 0.25 % Sim. to ISO 62
密度 1300 kg/m³ ISO 1183
密度 1300 kg/m³ ASTM D 792
材料特有の特性単位テスト基準
ISO データ
粘度数 160 cm³/g ISO 307, 1157, 1628
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 260 °C ISO 294
射出成形, 金型温度 60 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 - 120 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.04 % -
樹脂温度 250 - 275 °C -
金型温度 40 - 80 °C -
機能
 粘度せん断速度. , Ultradur® B 6550, PBT, BASF
 せん断応力-せん断速度. , Ultradur® B 6550, PBT, BASF
 応力-ひずみ. , Ultradur® B 6550, PBT, BASF
 割線弾性率−ひずみ. , Ultradur® B 6550, PBT, BASF
 応力-ひずみ (等時的). 23°C, Ultradur® B 6550, PBT, BASF
 クリープ弾性率−時間. 23°C, Ultradur® B 6550, PBT, BASF
クリープ曲線 23°C, Ultradur® B 6550, PBT, BASF
 引張弾性率-温度. , Ultradur® B 6550, PBT, BASF
特殊な特性
成形加工法.
射出成形., フィルム押出成形., 異形押出成形., シート押出成形., その他の押出成形.
納入形状.
ペレット., ナチュラルカラー
特殊な特性.
光安定化., 紫外線安定化., 熱安定化.
領域別の利用可能性
その他の情報
村遜速揃
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min
その他の押出成形.
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Prepreg, Melt temperature: 230 - 250 °C
Extrusion, Pipes, Melt temperature: 230 - 260 °C
Extrusion, cable sheathing, Melt temperature: 230 - 260 °C
族臓遜造揃
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Profiles, Melt temperature: 230 - 260 °C
促揃臓村促速揃
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Plates, Melt temperature: 230 - 250 °C
耐薬品性
5wt%酢酸 (23゚C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.