Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PET - PET - BASF

Material Data Center offers the following functions for Ultrafuse PET:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 16.3 cm³/10min ISO 1133
温度 220 °C -
荷重 2.16 kg -
熱的特性単位テスト基準
ISO データ
ガラス転移点, 10゚C/min 71 °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 61 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 63 °C ISO 75-1/-2
その他の特性.単位テスト基準
密度. 1330 kg/m³ ISO 1183
3D Data単位テスト基準
Other Standards[S]
引張弾性率, flat 1930 MPa ISO 527
引張弾性率, upright 1670 MPa ISO 527
引張強度, flat 33.4 MPa ISO 527
引張強度, upright 17.2 MPa ISO 527
破壊ひずみ, flat 2.7 % ISO 527
破壊ひずみ, upright 1.1 % ISO 527
曲げ弾性率, flat 2060 MPa ISO 178
曲げ弾性率, on-edge 1840 MPa ISO 178
曲げ弾性率, upright 1830 MPa ISO 178
曲げ強さ, flat 66.7 MPa ISO 178
曲げ強さ, on-edge 76.1 MPa ISO 178
曲げ強さ, upright 54.4 MPa ISO 178
シャルピー衝撃強さ, +23°C, flat 18.4 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, +23°C, on-edge 9.7 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, +23°C, upright 4.6 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C, flat 1.6 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, +23°C, on-edge 1.4 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, +23°C, upright 1.2 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C, flat 12.3 kJ/m² ISO 180/1U
アイゾット衝撃試験, +23°C, on-edge 7.7 kJ/m² ISO 180/1U
アイゾット衝撃試験, +23°C, upright 4.1 kJ/m² ISO 180/1U
ノッチ付きIzod衝撃強さ, +23°C, flat 2.1 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ, +23°C, on-edge 1.9 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ, +23°C, upright 1.8 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
特殊な特性
成形加工法.
Additive Manufacturing
納入形状.
Monofilament
な特性
Amorphous, Good Adhesion
領域別の利用可能性
北アメリカ., ヨーロッパ., 南・中央アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.