Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VECTRA® MT®1335 - (LCP+PTFE)-GF - Celanese

Material Data Center offers the following functions for VECTRA® MT®1335:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vectra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Vectra® MT1335 VF3001 (natural) is a glass/PTFE filled, tribologically-modified, easy flow LCP grade for injection molding.

Vectra® MT1335 VF3001 (natural) is a special grade developed for medical industry applications and complies with:
  • Food Contact Substance Notification (FCN) No. 742 of the Food and Drug Administration (FDA) and is listed in the Drug Master File (DMF 8464) and the Device Master File (MAF 315)
  • the corresponding EU and national registry regulatory requirements
  • biocompatibility in tests corresponding to USP 23 Class VI/ISO 10993
  • low residual monomers
  • no animal products
Best High Current Arc Ignition (HAI) performance
Chemical abbreviation according to ISO 1043-1 : LCP
Inherently flame retardant

Flammability at thickness hV-0-
Processing/Physical Characteristics単位テスト基準
ISO データ
成形収縮率, 平行 0.1 % ISO 294-4, 2577
成形収縮率, 直角 0.4 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 11000 MPa ISO 527
破壊応力 190 MPa ISO 527
破壊ひずみ 2.3 % ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 40 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 280 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 230 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 250 °C ISO 75-1/-2
ビカット軟化温度, B 146 °C ISO 306
線膨張係数, 直角 19 E-6/K ISO 11359-1/-2
厚さhでの燃焼性 V-0 class IEC 60695-11-10
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 3.5 - IEC 62631-2-1
比誘電率, 1MHz 3.1 - IEC 62631-2-1
誘電正接, 100Hz 200 E-4 IEC 62631-2-1
誘電正接, 1MHz 160 E-4 IEC 62631-2-1
体積抵抗率 1E13 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
耐電圧 32 kV/mm IEC 60243-1
その他の特性.単位テスト基準
密度 1620 kg/m³ ISO 1183
機能
 せん断弾性率-温度. , VECTRA® MT®1335, (LCP+PTFE)-GF, Celanese
 応力-ひずみ. , VECTRA® MT®1335, (LCP+PTFE)-GF, Celanese
 割線弾性率−ひずみ. , VECTRA® MT®1335, (LCP+PTFE)-GF, Celanese
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット., ナチュラルカラー
添加剤.
滑剤.
特殊な特性.
難燃., 光安定化., 滅菌可能, エチレンオキシド滅菌(EtO), 蒸気滅菌
な特性
Tribologic Grade
Certifications
Food contact, Food approval BfR, Food approval FDA 21 CFR, Food contact notification (FCN), Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved, Drug Master File, Device Master File
アプリケーション
医療の
領域別の利用可能性
北アメリカ., ヨーロッパ.
その他の情報
村遜速揃
Vectra resins are well known for their excellent thermal and hydrolytic stability. In order to ensure these properties are optimum, the resin should be dried correctly prior to processing. The Vectra MT-grades MT1300, MT1305, MT1310, MT1335, MT1340 and MT1345 should be dried at 150°C for a minimum of 4 hours in a desiccant dryer.
A three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed flights may be needed for smaller machines: 1/2 feed, 1/4 compression, 1/4 metering.

Vectra LCPs are shear thinning, their melt viscosity decreases quickly as shear rate increases. For parts that are difficult to fill, the molder can increase the injection velocity to improve melt flow.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.