Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Velocity® LCF40 - PA66 1 - PA66-CF40 - PlastiComp, Inc.

Material Data Center offers the following functions for Velocity® LCF40 - PA66 1:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Velocity datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
For more detailed information, please read our
or contact our representatives in your region.
機械的特性単位テスト基準
ASTM数据
引張弾性率 31030 MPa ASTM D 638
引張強度 296 MPa ASTM D 638
降伏点伸び 1.5 % ASTM D 638
曲げ弾性率 20680 MPa ASTM D 790
曲げ強さ 455 MPa ASTM D 790
ノッチ付きIzod衝撃強さ, 1/8 in 187 J/m ASTM D 256
アイゾット衝撃試験, 1/8 in 694 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 264 psi 252 °C ASTM D 648
その他の特性.単位テスト基準
密度 1310 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 85 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.18 % -
樹脂温度 293 - 310 °C -
金型温度 93 °C -
Zone 1 282 - 299 °C -
Zone 2 288 - 305 °C -
Zone 3 293 - 310 °C -
Nozzle temperature 288 - 305 °C -
Screw speed 30 - 50 rpm -
Injection speed 51 - 76 mm/s -
Back pressure 0.17 - 0.35 MPa -
特殊な特性
成形加工法.
射出成形.
な特性
Long fiber reinforced
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.