Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ML-GB30 - PA12-GB30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ML-GB30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Microglass bead-filled (30%) PA12 resin for the injection moulding of rigid, low-warpage and dimensionally accurate mouldings

 

Biocompatibility of VESTAMID® Care ME

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation


Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 



The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY

 

Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 100 / * cm³/10min ISO 1133
温度 275 / * °C -
荷重 5 / * kg -
成形収縮率, 平行 0.6 / * % ISO 294-4, 2577
成形収縮率, 直角 0.7 / * % ISO 294-4, 2577
溶融時の密度 1090 kg/m³ -
溶融時の熱伝導率 0.28 W/(m K) -
溶融時の比熱 2400 J/(kg K) -
突き出し時の時の温度 180 °C -
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 2100 / 1800 MPa ISO 527
降伏応力 47 / 37 MPa ISO 527
降伏ひずみ 5 / 5 % ISO 527
破壊呼びひずみ 20 / >50 % ISO 527
引張クリープ弾性率, 1h * / 1600 MPa ISO 899-1
引張クリープ弾性率, 1000h * / 1100 MPa ISO 899-1
シャルピー衝撃強さ, +23°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
シャルピー衝撃強さ, -30°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
ノッチ付きシャルピー衝撃強さ, +23°C 4.4 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
ノッチ付きシャルピー衝撃強さ, -30°C 6 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 178 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 55 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 150 / * °C ISO 75-1/-2
ビカット軟化温度, B 155 / * °C ISO 306
線膨張係数, 平行 130 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 130 / * E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 1.6 / * mm -
電気的特性.乾燥/調湿単位テスト基準
ISO データ
比誘電率, 100Hz 4.1 / 5 - IEC 62631-2-1
比誘電率, 1MHz 3.5 / 4 - IEC 62631-2-1
誘電正接, 100Hz 310 / 600 E-4 IEC 62631-2-1
誘電正接, 1MHz 230 / 370 E-4 IEC 62631-2-1
体積抵抗率 >1E13 / 2E12 Ohm*m IEC 62631-3-1
表面抵抗率 * / 1E15 Ohm IEC 62631-3-2
耐電圧 - / 36 kV/mm IEC 60243-1
耐トラッキング性 600 / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 1.1 / * % Sim. to ISO 62
吸湿率 0.5 / * % Sim. to ISO 62
密度 1250 / 1260 kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 250 °C ISO 294
射出成形, 金型温度 80 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
射出成形, 保圧 70 MPa ISO 294
機能
 粘度せん断速度. , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
 せん断応力-せん断速度. , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
 せん断弾性率-温度. , VESTAMID® Care ML-GB30 (乾燥), PA12-GB30, Evonik
 応力-ひずみ. , VESTAMID® Care ML-GB30 (乾燥), PA12-GB30, Evonik
 割線弾性率−ひずみ. , VESTAMID® Care ML-GB30 (乾燥), PA12-GB30, Evonik
 応力-ひずみ (等時的). 23°C, VESTAMID® Care ML-GB30 (調湿), PA12-GB30, Evonik
 クリープ弾性率−時間. 23°C, VESTAMID® Care ML-GB30 (調湿), PA12-GB30, Evonik
クリープ曲線 23°C, VESTAMID® Care ML-GB30 (調湿), PA12-GB30, Evonik
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
な特性
Low Warpage
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
アプリケーション
医療の
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com