Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® E62-S3 BK V303579 - TPA - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® E62-S3 BK V303579:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Heat- and light-stabilized compound based on polyamide 12 elastomer for molding of sport shoe soles

VESTAMID® E62-S3 BK V303579 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer.

The VESTAMID® E represent thermoplastic elastomers generically characterized as polyether block copolyamides (PEBA) consisting of PA 12 and polyether segments.

VESTAMID® E62-S3 BK V303579 is especially developed for sport shoe soles. It has good impact strength at low temperatures.

VESTAMID® E62-S3 BK V303579 is supplied as cylindrical pellets in moisture-proof packaging, ready for processing.
 
The process temperatures should be within a range of 190°C – 230°C.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 9 / * cm³/10min ISO 1133
温度 230 / * °C -
荷重 2.16 / * kg -
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 405 / - MPa ISO 527
降伏応力 24 / - MPa ISO 527
降伏ひずみ 30 / - % ISO 527
破壊呼びひずみ >50 / - % ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 95 / - kJ/m² ISO 179/1eA
ショア硬さD 61 / * - ISO 7619-1
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 171 / * °C ISO 11357-1/-3
特殊な特性
納入形状.
ペレット., 黒
特殊な特性.
光安定化., 熱安定化.
な特性
Copolymer
アプリケーション
スポーツ用品
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.