Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAPE® PA12-CF45 20641 - PA12-CF45 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAPE® PA12-CF45 20641:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Vestape datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
HT carbon fiber reinforced UD-tape made from polyamide 12 

VESTAPE® PA12-CF45 is an unidirectional carbon fiber reinforced tape made from PA12 with a fiber volume content of 45 %, that shows a high chemical resistance, low water absorption and steady mechanical properties over a wide temperature range.

VESTAPE® PA12-CF45  is supplied as a band-shaped semi-finished product showing a width of 160 mm and a thickness of 0,25 mm.


Further information about the properties and the processing of VESTAPE® can be found in our brochure „VESTAPE“.
 


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCTS AT COMPOSITES.EVONIK.COM.
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 178 °C ISO 11357-1/-3
ガラス転移点, 10°C/min 40 °C ISO 11357-1/-2
その他の特性.単位テスト基準
吸湿率 0.47 % Sim. to ISO 62
密度 1360 kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
金型温度, of test plate 220 °C -
成形時間, of test plate 5 min -
冷却速度, of test plate 20 K/min -
成形品取出温度, of test plate 40 °C -
成形圧力, of test plate 1 MPa -
特殊な特性
成形加工法.
熱成形.
納入形状.
Tape
特殊な特性.
導電., 熱安定化.
耐薬品性
General Chemical Resistance
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.