Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTORAN® 1900 GF20 HE30018 - PPE-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTORAN® 1900 GF20 HE30018:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestoran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Modified polyphenylene ether (PPE), heat resistant, glass fiber-reinforced, suitable for K K process

VESTORAN® 1900GF20 HE30018 is the registered trademark of Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (polyphenylene ether, PPE, also referred to as PPO).

As a material of amorphous structure VESTORAN® 1900GF20 HE30018 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp.

Moldings of VESTORAN® 1900GF20 HE30018 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics.

VESTORAN® 1900GF20 HE30018 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions.

Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity.

VESTORAN®1900GF20 HE30018 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites patented K&K process ("direct-bonding to rubber").
 
VESTORAN® 1900GF20 HE30018 is supplied as cylindrical granules in polyethylene packaging.
 
Pigmentation may affect values.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 45 cm³/10min ISO 1133
温度 300 °C -
荷重 21.6 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 5700 MPa ISO 527
破壊応力 103 MPa ISO 527
破壊ひずみ 2 % ISO 527
シャルピー衝撃強さ, +23°C 45 kJ/m² ISO 179/1eU
Type of failure C - -
ノッチ付きシャルピー衝撃強さ, +23°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 190 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 195 °C ISO 75-1/-2
ビカット軟化温度, B 195 °C ISO 306
線膨張係数, 平行 40 E-6/K ISO 11359-1/-2
線膨張係数, 直角 50 E-6/K ISO 11359-1/-2
その他の特性.単位テスト基準
密度 1200 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
熱安定化.
な特性
Amorphous, Good Adhesion, Low Warpage
耐薬品性
Acid Resistance, Alkali Resistance, Hydrolytically Stable
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com