Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 21SPC - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 21SPC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Vydyne 21SPC is a general-purpose, unfilled, lubricated, PA66 resin. Designed principally for injection-molding fabrication, this product offers a combination of engineering properties characterized by high strength; rigidity; good toughness; high melt point; good surface lubricity; abrasion resistance; and resistance to many chemicals, machine and motor oils, solvents and gasoline.

21SPC permits production of molded parts with good initial color plus good property and color retention when using regrind.

21SPC is intended for use in high-productivity applications. In many applications, the molding cycle can be reduced because parts may be removed from the cavity at higher temperatures. In difficult molds where parts have a tendency to stick in the cavity, 21SPC can reduce or eliminate the need for mold release sprays. Critical molded-part dimensions should be checked against specifications before implementing shorter molding cycles on a routine production basis.

Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
成形収縮率, 平行 1.8 / * % ISO 294-4, 2577
成形収縮率, 直角 1.7 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 2800 / 1800 MPa ISO 527
降伏応力 86 / 56 MPa ISO 527
降伏ひずみ 4.8 / 22 % ISO 527
シャルピー衝撃強さ, +23°C N / N kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C N / N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 6 / 20 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 5 / 7 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 260 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 70 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 200 / * °C ISO 75-1/-2
線膨張係数, 平行 100 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 100 / * E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 V-2 / * class IEC 60695-11-10
試験片の厚さ 1.5 / * mm -
厚さhでの燃焼性 V-2 / * class IEC 60695-11-10
試験片の厚さ 0.4 / * mm -
酸素指数 25 / * % ISO 4589-1/-2
電気的特性.乾燥/調湿単位テスト基準
ISO データ
体積抵抗率 1E11 / - Ohm*m IEC 62631-3-1
耐電圧 26 / - kV/mm IEC 60243-1
耐トラッキング性 600 / - - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 1.2 / * % Sim. to ISO 62
吸湿率 2.4 / * % Sim. to ISO 62
密度 1140 / - kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット., ナチュラルカラー
添加剤.
滑剤., 離型剤.
耐薬品性
General Chemical Resistance, Solvent Resistance, Oil Resistance
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Drinking water contact, Drinking water contact NSF 61
アプリケーション
自動車, 電気電子, 汎用
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.