Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R433H BK0746 - PA66-GF33 - Ascend

Material Data Center offers the following functions for Vydyne® R433H BK0746:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Vydyne R433H BK0746 is designed to reinforce downgauged steel and aluminum used in vehicle body-in-white (BIW) structures, helping reduce weight without sacrificing safety or comfort.
R433H BK0746 has improved energy absorption over traditional glass-filled PA66, helping reduce noise, vibration and harshness (NVH) and absorbing impact energy from crashes. Using R433H BK0746 in the BIW structure reinforces sheet metal, helping manufacturers shave substantial weight and improve efficiency. Trends in lightweight and NVH are becoming even more paramount with the growth of Electric Vehicles. Vydyne R433H BK0746 has excellent performance attributes to support applications where this will be of prime importance such as battery frames and housings.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
成形収縮率, 平行 0.6 / * % ISO 294-4, 2577
成形収縮率, 直角 1.0 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 9600 / 6200 MPa ISO 527
降伏応力 150 / 103 MPa ISO 527
降伏ひずみ 3.3 / 7.4 % ISO 527
曲げ弾性率, 23°C 8400 / 6000 MPa ISO 178
曲げ強さ 210 / 130 MPa ISO 178
シャルピー衝撃強さ, +23°C 96 / 96 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 100 / 92 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 24 / 27 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 17 / 16 kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C 21 / 29 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ 15 / - kJ/m² ISO 180/1A
温度 -40 °C -
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 262 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 245 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 260 / * °C ISO 75-1/-2
線膨張係数, 平行 16 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 11 / * E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 1.5 / * mm -
厚さhでの燃焼性 V-2 / * class IEC 60695-11-10
試験片の厚さ 0.4 / * mm -
ASTM数据
UL94 燃焼性 V-2 - UL 94
追加試験片の厚さ 0.4 mm -
電気的特性.乾燥/調湿単位テスト基準
ISO データ
耐電圧 28 / - kV/mm IEC 60243-1
その他の特性.乾燥/調湿単位テスト基準
吸水率 1 / * % Sim. to ISO 62
吸湿率 1.3 / * % Sim. to ISO 62
密度 1350 / - kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
樹脂温度 285 - 305 °C -
金型温度 65 - 95 °C -
Zone 1 280 - 310 °C -
Zone 2 280 - 310 °C -
Zone 3 280 - 310 °C -
Nozzle temperature 280 - 310 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット., 黒
添加剤.
滑剤.
特殊な特性.
高耐衝撃及び耐衝撃改良., 熱安定化.
な特性
Acoustical Barrier Properties
耐薬品性
General Chemical Resistance, Solvent Resistance, Oil Resistance
アプリケーション
自動車, カプセル化された
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.