Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of XAREC® C 142 - (PS-SY)-GF40 - Idemitsu Chemicals

Material Data Center offers the following functions for XAREC® C 142:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Xarec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
成形収縮率, 平行 0.2 % ISO 294-4, 2577
成形収縮率, 直角 0.7 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 12600 MPa ISO 527
破壊応力 130 MPa ISO 527
破壊ひずみ 1.5 % ISO 527
曲げ弾性率, 23°C 12400 MPa ISO 178
曲げ強さ 195 MPa ISO 178
シャルピー衝撃強さ, +23°C 27 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 9 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C 33 kJ/m² ISO 180/1U
ノッチ付きIzod衝撃強さ, +23°C 10 kJ/m² ISO 180/1A
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 250 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 270 °C ISO 75-1/-2
線膨張係数, 平行 15 E-6/K ISO 11359-1/-2
線膨張係数, 直角 40 E-6/K ISO 11359-1/-2
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 0.8 mm -
Yellow Card 可用 はい - -
電気的特性.単位テスト基準
ISO データ
耐トラッキング性 500 - IEC 60112
ASTM数据
耐電圧, 短い時間 45 kV/mm ASTM D 149
耐アーク 90 s ASTM D 495
Other Standards[S]
比誘電率, 1MHz 3 - IEC 60250
誘電正接, 1MHz 10 E-4 IEC 60250
体積抵抗率 1E14 Ohm*m IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
密度. 1360 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 5 h -
樹脂温度 280 - 310 °C -
金型温度 130 - 155 °C -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
高耐衝撃及び耐衝撃改良.
アプリケーション
電気電子
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com