Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Adsyl 5 C 39 F - PP - LyondellBasell Industries

Material Data Center offers the following functions for Adsyl 5 C 39 F:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Adsyl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 5.5 g/10min ISO 1133
温度 230 °C -
荷重 2.16 kg -
熱的特性単位テスト基準
ISO データ
溶融温度, 10゚C/min 132 °C ISO 11357-1/-3
荷重たわみ温度, 0.45 MPa 62 °C ISO 75-1/-2
ビカット軟化温度, A 107 °C ISO 306
光学特性単位テスト基準
ASTM数据
光沢度 87 - ASTM D 2457
ヘイズ 1.2 % ASTM D 1003
その他の特性.単位テスト基準
密度. 900 kg/m³ ISO 1183
機械的特性(ィルム)単位テスト基準
ISO データ
引張弾性率, 平行 280 MPa ISO 527-3
引張弾性率, 直角 280 MPa ISO 527-3
降伏応力, 平行 14 MPa ISO 527-3
降伏応力, normal 14 MPa ISO 527-3
降伏ひずみ, 平行 17 % ISO 527-3
降伏ひずみ, n直角 15 % ISO 527-3
破壊応力, 平行 45 MPa ISO 527-3
破壊応力, 直角 35 MPa ISO 527-3
最大ひずみ, 平行 900 % ISO 527-3
最大ひずみ, 直角 800 % ISO 527-3
押出成形のタイプ. cast - -
試験片の厚さ. 0.05 mm -
特殊な特性
成形加工法.
フィルム押出成形.
添加剤.
ブロッキング防止剤.
な特性
Heat Sealable
Certifications
Food contact, Food approval 1935/2004/EC, Food approval 10/2011, Food approval FDA 21 CFR
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.