Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Altuglas® CR 8 - PMMA - Altuglas International

Material Data Center offers the following functions for Altuglas® CR 8:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Altuglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 0.7 g/10min ISO 1133
温度 230 °C -
荷重 3.8 kg -
ASTM数据
成形収縮率., 平行 0.005 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張強度 45 MPa ISO 527
破壊ひずみ 35 % ISO 527
曲げ弾性率, 23°C 2200 MPa ISO 178
シャルピー衝撃強さ, +23°C 45 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 4 kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C 4.5 kJ/m² ISO 180/1A
ASTM数据
ロックウェル硬度 M 74 - ASTM D 785
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 90 °C ISO 75-1/-2
ビカット軟化温度, B 101 °C ISO 306
ASTM数据
UL94 燃焼性 HB - UL 94
線膨張係数, 平行 90 E-6/K ASTM D 696
電気的特性.単位テスト基準
ASTM数据
耐電圧, 短い時間 16.5 kV/mm ASTM D 149
誘電正接, 1 MHz 0.04 - ASTM D 150
比誘電率, 60 Hz 3.85 - ASTM D 150
表面抵抗率 1E14 Ohm ASTM D 257
体積抵抗率 >1E15 Ohm*cm ASTM D 257
光学特性単位テスト基準
ASTM数据
ヘイズ 1.5 % ASTM D 1003
視感透過率 91 % ASTM D 1003
その他の特性.単位テスト基準
吸湿率 0.34 % Sim. to ISO 62
密度. 1160 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 85 °C -
Pre-drying - Time 4 h -
樹脂温度 235 - 245 °C -
金型温度 80 - 90 °C -
特殊な特性
成形加工法.
射出成形.
特殊な特性.
透明.
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.