Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bayblend® T88 GF-30 - (PC+SAN)-I-GF30 - Covestro Deutschland AG

Material Data Center offers the following functions for Bayblend® T88 GF-30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Bayblend datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
  • Rubber modified (PC SAN) blend
  • 31 % glass fiber filled
  • Vicat/B 120 temperature = 134 °C
  • optimized heat ageing- and UV-stability
  • very good flow
  • tensile modulus = 10000 MPa
  • good heat resistance
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 11 cm³/10min ISO 1133
温度 260 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 10000 MPa ISO 527
破壊応力 135 MPa ISO 527
破壊ひずみ 2 % ISO 527
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 126 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 134 °C ISO 75-1/-2
ビカット軟化温度, B 132 °C ISO 306
線膨張係数, 平行 25 E-6/K ISO 11359-1/-2
線膨張係数, 直角 60 E-6/K ISO 11359-1/-2
厚さhでの燃焼性 HB class IEC 60695-11-10
試験片の厚さ 0.8 mm -
電気的特性.単位テスト基準
ISO データ
比誘電率, 100Hz 3.6 - IEC 62631-2-1
比誘電率, 1MHz 3.4 - IEC 62631-2-1
誘電正接, 100Hz 30 E-4 IEC 62631-2-1
誘電正接, 1MHz 85 E-4 IEC 62631-2-1
体積抵抗率 >1E13 Ohm*m IEC 62631-3-1
表面抵抗率 >1E15 Ohm IEC 62631-3-2
耐電圧 35 kV/mm IEC 60243-1
耐トラッキング性 175 - IEC 60112
その他の特性.単位テスト基準
吸水率 0.4 % Sim. to ISO 62
吸湿率 0.1 % Sim. to ISO 62
密度 1380 kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 260 °C ISO 294
射出成形, 金型温度 80 °C ISO 294
射出成形, 射出速度 540 mm/s ISO 294
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 100 - 110 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
樹脂温度 240 - 280 °C -
金型温度 70 - 100 °C -
機能
 粘度せん断速度. , Bayblend® T88 GF-30, (PC+SAN)-I-GF30, Covestro
 せん断応力-せん断速度. , Bayblend® T88 GF-30, (PC+SAN)-I-GF30, Covestro
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
離型剤.
特殊な特性.
高耐衝撃及び耐衝撃改良., 熱安定化.
領域別の利用可能性
その他の情報
村遜速揃
PREPROCESSING
Max. Water content: 0.02 %
Drying temperature: 100 - 110 °C
(depending on the grade 10°C below the Vicat VST/B120 temperature, but not higher as the recommended values).
Drying time:
Circulating air drying oven (50 % fresh air) 4-8 h
Fresh air dryer (high speed dryer) 2-4 h
Dry air dryer 2-4 h

PROCESSING
Melt temperature: 240-280 °C
Mold temperature: 70-100 °C

Use open nozzle.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com