Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CirculenRecover HD5603 Silver - (PE-HD) - LyondellBasell Industries

Material Data Center offers the following functions for CirculenRecover HD5603 Silver:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Circulen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
CirculenRecover HD5603 Silver contains at least 98% of recycled material.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 0.4 g/10min ISO 1133
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 1200 MPa ISO 527
降伏応力 24 MPa ISO 527
降伏ひずみ 9 % ISO 527
ノッチ付きシャルピー衝撃強さ, -30゚C 2.5 kJ/m² ISO 179/1eA
その他の特性.単位テスト基準
密度. 956 kg/m³ ISO 1183
Bulk density 500 kg/m³ -
Processing Recommendation Extrusion単位テスト基準
樹脂温度 180 - 210 °C -
特殊な特性
成形加工法.
異形押出成形., シート押出成形., ブロー成形.
納入形状.
ペレット.
耐薬品性
Oxidation Resistance
Certifications
Recycled Resin Content
アプリケーション
汎用, パッケージング
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.