Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ Renew 401-50 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ Renew 401-50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastman Cristal™ Renew 401-50 copolyester is a high flow product that contains mold release for ease of ejection.

It is designed and engineered specifically for cosmetics packaging applications. With its unsurpassed color and

clarity and an unmatched ability to mold thick parts with improved gate aesthetics, Cristal 401-50 Renew is clearly

a well-suited copolyester for premium cosmetics packaging. Other outstanding features of Cristal™ Renew 401-50

copolyester are excellent chemical resistance, high gloss, and improvements in processing such as faster cycle

times, and lower scrap rates. Cristal Renew 401-50 is also ideally suited for two-shot molding techniques due to

its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a

global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are

produced with ISCC certified circular content by mass balance allocation.


Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.0035 mm/mm ASTM D 955
機械的特性単位テスト基準
ISO データ
引張弾性率 2030 MPa ISO 527
降伏応力 50 MPa ISO 527
降伏ひずみ 4.3 % ISO 527
破壊応力 20 MPa ISO 527
破壊ひずみ 39 % ISO 527
ASTM数据
引張弾性率 2036 MPa ASTM D 638
降伏応力 50 MPa ASTM D 638
破壊応力 24 MPa ASTM D 638
降伏点伸び 4.4 % ASTM D 638
破断伸び 44 % ASTM D 638
曲げ弾性率 1808 MPa ASTM D 790
曲げ強さ 66 MPa ASTM D 790
ロックウェル硬度 R 108 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 103 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 44 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 68 °C ASTM D 648
DTUL @ 264 psi 61 °C ASTM D 648
光学特性単位テスト基準
ASTM数据
ヘイズ 0.4 % ASTM D 1003
視感透過率 91.8 % ASTM D 1003
その他の特性.単位テスト基準
密度 1280 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 65 °C -
Pre-drying - Time 8 h -
樹脂温度 205 - 240 °C -
金型温度 16 - 38 °C -
特殊な特性
成形加工法.
射出成形., その他の押出成形.
納入形状.
ナチュラルカラー
添加剤.
離型剤.
特殊な特性.
高耐衝撃及び耐衝撃改良., 透明.
な特性
High Gloss, Copolymer
耐薬品性
General Chemical Resistance
Certifications
ISCC Plus
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.