Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ AN014-30 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ AN014-30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文

Eastar™ Renew copolyester AN014-30 Natural is a high flow product that contains mold release. Other features include excellent appearance and clarity, good physical properties, chemical resistance, and ease of melt processing with an increase of 20-40% in flow length over copolyester AN004-30 Natural, as determined by spiral

flow testing. This high flow product is especially suited for those applications utilizing thin-walled intricate tools.

Eastar™ Renew copolyester AN014-30 Natural is approved for food contact and thereby under existing United States Food and Drug Administration (FDA) regulations, it may be used in food contact articles which comply with

the specifications and conditions of use in 21 CFR 177.1240.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Renew polymers enable a brand to reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.

Processing/Physical Characteristics単位テスト基準
ASTM数据
成形収縮率., 平行 0.003 mm/mm ASTM D 955
機械的特性単位テスト基準
ASTM数据
降伏応力 50 MPa ASTM D 638
破壊応力 43 MPa ASTM D 638
降伏点伸び 5 % ASTM D 638
破断伸び 270 % ASTM D 638
曲げ弾性率 1900 MPa ASTM D 790
ロックウェル硬度 R 107 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 80 J/m ASTM D 256
ノッチ付きIzod衝撃強さ, Low-Temperature 44 J/m ASTM D 256
温度 -40 °C -
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 73 °C ASTM D 648
DTUL @ 264 psi 66 °C ASTM D 648
ビカット軟化温度 86 °C ASTM D 1525
光学特性単位テスト基準
ASTM数据
ヘイズ 1 % ASTM D 1003
視感透過率 92 % ASTM D 1003
その他の特性.単位テスト基準
吸水率, 24hr 0.15 % ASTM D 570
密度 1190 kg/m³ ASTM D 792
Processing Recommendation Extrusion単位テスト基準
Pre-drying - Temperature 70 °C -
Pre-drying - Time 4 h -
樹脂温度 230 - 280 °C -
金型温度 15 - 30 °C -
特殊な特性
成形加工法.
異形押出成形.
納入形状.
ナチュラルカラー
添加剤.
離型剤.
特殊な特性.
透明.
な特性
Copolymer
耐薬品性
General Chemical Resistance
Certifications
Food contact, Food approval FDA 21 CFR, ISCC Plus
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.